Refractory Metals and Alloys
| Physical Properties | UNIT | Molybdenum | TZM Molybdenum | Tantalum | Niobium | Tungsten | Rhenium |
|---|---|---|---|---|---|---|---|
| Density | lb/cu in | 0.369 | 0.37 | 0.6 | 0.31 | 0.7 | 0.77 |
| Density | gm/cm3 | 10.30 | 10.22 | 16.6 | 8.57 | 19.30 | 21.20 |
| Melting Point | °F | 4760 | 4753 | 5425 | 4380 | 6170 | 5767 |
| Melting Point | °C | 2625 | 2623 | 2996 | 2415 | 3410 | 3180 |
| Electrical Resistivity | micro-ohm-cm | 5.17 | 6.85 | 12.40 | 13.10 | 5.5 | 13.5 |
| Thermal Conductivity | cal/cm2/cm°C/sec | 0.35 | 0.30 | 0.13 | - | 0.48 | 0.39 |
| Specific Heat | Cal/gm/°C | 0.061 | 0.073 | 0.036 | 0.065 | 0.032 | 0.033 |
| Recrystalization Temp. | °C | 1100 | 1400 | - | 800 | - | - |
| Coefficient of | in/in/°F x 106 | 4.9 | 4.9 | 6.5 | 7.1 | 4.3 | 6.32 |
| Linear Thermal Expansion | m/m/°K/ x 106 | 4.8 | 4.8 | 6.3 | 7.3 | 4.6 | 6.80 |
| Mechanical Properties | UNIT | Molybdenum | TZM Molybdenum | Tantalum | Niobium | Tungsten | Rhenium |
|---|---|---|---|---|---|---|---|
| Tensile Strength | KSI (Mpa)-RT | 150 (1035) | 110 (750) | 50 (345) | 40 (275) | 250 (1725) | 200 (1380) |
| Tensile Strength | KSI (Mpa)-500°C | 75 (515) | - | 35 (240) | 30 (205) | 150 (1035) | 135 (930) |
| Tensile Strength | KSI (Mpa)-1000°C | 25 (175) | - | 15 (100) | 10 (70) | 75 (515) | 70 (480) |
| Elongation | %(in.) 1.0" | 12 | 15 | 20 | 30 | - | 2 |
| Typical Hardness | DPH (vickers) RC | 230 | 220 | 200 | 130 | 300 | - |
| Modulus of Elasticity | ksi | 45,000 | 48,000 | 27,000 | 15,250 | 58,000 | 67,150 |
| Modulus of Elasticity | Gpa | 310 | 320 | 185 | 105 | 400 | 483 |
| Chemistry | UNIT | Molybdenum | TZM Molybdenum | Tantalum | Niobium | Tungsten | Rhenium |
|---|---|---|---|---|---|---|---|
| minimum % | - | 99.95 Mo | 99.20 Mo | 98.99 Ta | 99.6 Nb | 99.95 W | 99.97 Re |
| minimum % | - | - | 0.08 - 0.12 Zn | - | - | - | - |
| minimum % | - | - | 0.40 - 0.50 Ti | - | - | - | - |
| Specifications | Molybdenum | TZM Molybdenum | Tantalum | Niobium | Tungsten | Rhenium |
|---|---|---|---|---|---|---|
| ASTM | B386 type 361 | B386 type 364 | B365 | B392 | - | - |
| ASTM | B387 type 361 | B387 type 364 | - | B393 | - | - |
| AMS | 7800 | 7817 | 7849 | 7850 | 7898/7899 | - |
| ASTM-B-777 | Class 1 Non-magnetic | Class 1 Magnetic | Class 2 | Class 3 Non-magnetic | Class 3 Magnetic | Class 4 |
|---|---|---|---|---|---|---|
| Chemistry | 90% W 6% Ni 4% Cu | 90% W 7% Ni 3% Fe | 92.5% W 5.25% Ni 2.25% Fe | 95% W 3.5% Ni 1.5% Cu | 95% W 3.5% Ni 1.5% Fe | 97% W 2.1% Ni .9% Fe |
| Density Gms/cc | 17 | 17 | 17.5 | 18 | 18 | 18.5 |
| Density Lbs/cu. in. | 0.614 | 0.614 | 0.632 | 0.65 | 0.65 | 0.668 |
| Hardness Rockwell C | 24 | 25 | 26 | 27 | 27 | 28 |
| Ultimate Tensile Strength (PSI) | 110,000 | 125,000 | 114,000 | 115,000 | 125,000 | 128,000 |
| Yield Strength .2% offset (PSI) | 90,000 | 88,000 | 90,000 | 85,000 | 90,000 | 85,000 |
| Elongation (% in 1") | 8 | 14 | 12 | 7 | 12 | 10 |
| Proportional Elastic Limit (PSI) | 45,000 | 52,000 | 46,000 | 45,000 | 44,000 | 45,000 |
| Modules of Elasticity (PSI) | 40 x 106 | 45 x 106 | 47 x 106 | 45 x 106 | 50 x 106 | 53 x 106 |
| Coefficient of Thermal Expansion X 10-6/°C (20-400°C) | 5.4 | 4.8 | 4.6 | 4.4 | 4.6 | 4.5 |
| Thermal Conductivity (CGS Units) | 0.23 | 0.18 | 0.2 | 0.33 | 0.26 | 0.3 |
| Electrical Conductivity (% IACS) | 14 | 10 | 13 | 16 | 13 | 17 |
| Magnetic Permeability (μ) | >1.05 | <1.05 | >1.05 | >1.05 | <1.05 | >1.05 |
We’re one of Europe’s leading suppliers of premium quality refractory metals and alloys, soft magnetic alloys, and controlled expansion alloys. Download this Linecard to see our range of stock materials: